Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.320 - 0.350 g/cc | 0.0116 - 0.0126 lb/in³ | |
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1â€) upwards. F.. |
|||
Density | 0.290 - 0.350 g/cc | 0.0105 - 0.0126 lb/in³ | True, 3M QCM 14.24.6 |
3M HGS2000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.290 - 0.350 g/cc | 0.0105 - 0.0126 lb/in³ | |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |