Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.290 - 0.310 g/cc | 0.0105 - 0.0112 lb/in³ | Free Density |
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |