Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 170R Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0250 - 0.100 g/cc | 0.000903 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 270R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0300 - 0.100 g/cc | 0.00108 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 340R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0300 - 0.100 g/cc | 0.00108 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 350R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0350 - 0.100 g/cc | 0.00126 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 370R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0190 - 0.100 g/cc | 0.000686 - 0.00361 lb/in³ | Pressurized batch pre-foamer; Usual Use |
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an.. |
|||
Density | 0.0500 - 0.100 g/cc | 0.00181 - 0.00361 lb/in³ | Normal molded density |
NOVA Chemicals Styrocell® D833A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |
|||
Density | 0.0800 - 0.100 g/cc | 0.00289 - 0.00361 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 100 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0600 - 0.100 g/cc | 0.00217 - 0.00361 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-S EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1702 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1710 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1710 120 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1710 50 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1710 60 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1712 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0100 - 0.100 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.00361 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® 1710 40 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Density | 0.0700 - 0.100 g/cc | 0.00253 - 0.00361 lb/in³ | Normal molded density |
NOVA Chemicals Styrocell® D933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |
|||
Density | 0.0800 - 0.100 g/cc | 0.00289 - 0.00361 lb/in³ | |
Sinotek Materials Soft Graphite Ring Used for electrode joint.Information provided by Sinotek |