Physical Properties Metric English Comments
Density 0.0800 - 0.0900 g/cc
0.00289 - 0.00325 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..