Polymer Property : Density = 0.0870 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0580 - 0.0870 g/cc
0.00210 - 0.00314 lb/in³
sheet density
Zotefoams Plastazote® HD80 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..