Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0220 - 0.0800 g/cc | 0.000795 - 0.00289 lb/in³ | |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Density | 0.0200 - 0.0800 g/cc | 0.000723 - 0.00289 lb/in³ | |
Polimeri Europa Extir® EH 3000 Expandable Polystyrene Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u.. |
|||
Density | 0.0150 - 0.0800 g/cc | 0.000542 - 0.00289 lb/in³ | |
BASF Styropor® BFL 322 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Density | 0.0170 - 0.0800 g/cc | 0.000614 - 0.00289 lb/in³ | |
Polimeri Europa Extir® EH 5000 Expandable Polystyrene Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i.. |
|||
Density | 0.0300 - 0.0800 g/cc | 0.00108 - 0.00289 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova W441A Expandable Polystyrene A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for.. |
|||
Density | 0.0400 - 0.0800 g/cc | 0.00145 - 0.00289 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Density | 0.0400 - 0.0800 g/cc | 0.00145 - 0.00289 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA.. |