Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0100 - 0.0250 g/cc | 0.000361 - 0.000903 lb/in³ | |
Polimeri Europa Extir® LN 5000 Expandable Polystyrene Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e.. |
|||
Density | 0.0150 - 0.0250 g/cc | 0.000542 - 0.000903 lb/in³ | Normal range, one pre-expansion |
SABIC EPS 650FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal range, one pre-expansion |
SABIC EPS 652 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Density | 0.0150 - 0.0250 g/cc | 0.000542 - 0.000903 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 65XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product for molding blocks of average and low densities.Informati.. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0100 - 0.0250 g/cc | 0.000361 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 5000 Expandable Polystyrene, Standard
(discontinued **) Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 9 g/l. Minimum apparent density on a discontinuous pre-expander is 13 g/l.Processing technology used for Type A.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova Styrocell® M442C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4.. |
|||
Density | 0.0130 - 0.0250 g/cc | 0.000470 - 0.000903 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.0140 - 0.0250 g/cc | 0.000506 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure.. |
|||
Density | 0.0140 - 0.0250 g/cc | 0.000506 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent.. |
|||
Density | 0.0190 - 0.0250 g/cc | 0.000686 - 0.000903 lb/in³ | sheet density |
Zotefoams Plastazote® LD23 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0190 - 0.0250 g/cc | 0.000686 - 0.000903 lb/in³ | sheet density |
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0190 - 0.0250 g/cc | 0.000686 - 0.000903 lb/in³ | sheet density |
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0190 - 0.0250 g/cc | 0.000686 - 0.000903 lb/in³ | sheet density |
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |