Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.97 g/cc | 0.360 lb/in³ | |
Indium Corp. Indalloy 48 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.97 g/cc | 0.360 lb/in³ | |
Indium Corp. Indalloy® 10 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Density | 9.97 g/cc | 0.360 lb/in³ | |
Williams Advanced Alloys WS264 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |