Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.42 g/cc | 0.340 lb/in³ | |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Density | 9.42 g/cc | 0.340 lb/in³ | |
Lucas-Milhaupt BRAZE 560 Characteristics:Braze 560 is a low temperature, free-flowing brazing filler metal with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through it.. |