Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.99 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
Lucas-Milhaupt BRAZE 401 Characteristics:Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc .. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy® 97 Pb-Sn-Bi Solder Alloy Good general purpose step soldering alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire. |