Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.89 g/cc | 0.321 lb/in³ | |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | at RT |
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Plate Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 0% Cold Work (Annealed) Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed tubing. Other property values are typical of INCO® C276.Data provided by the manufacturer, Speci.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 201 Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)... |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/2 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/8 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 3/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, Annealed Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, Full Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
CMW® 28 Copper Alloy CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness t.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Cadi 150 Copper Alloy A small addition of Zr to copper improves resistance to softening and resists deformation at high temperatures where normal copper would soften rapidly. Zirconium copper is used as a Class 1 electr.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 60 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Alloy Wire International RW 45 Ni-Cu Resistance Wire Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International. |