Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types .. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Annealed Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ AT Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Indium Corp. Indalloy 219 Ag-Au-Zn-Cd Solder Alloy Information Provided by Indium Corporation |