Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.65 g/cc | 0.313 lb/in³ | |
CLAL-MSX NICLAL 1300 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Density | 8.65 g/cc | 0.313 lb/in³ | |
CLAL-MSX NICLAL 1300 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
Density | 8.65 g/cc | 0.313 lb/in³ | |
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |