Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.287 g/cc | 0.2994 lb/in³ | |
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |
|||
Density | 8.287 g/cc | 0.2994 lb/in³ | |
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |
|||
Density | 8.287 g/cc | 0.2994 lb/in³ | |
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |