Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed Only |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Density | 8.27 g/cc | 0.299 lb/in³ | Solution Annealed |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |