Polymer Property : Density = 8.193 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.193 g/cc
0.2960 lb/in³
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS)
CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal..