Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.00 g/cc | 0.289 lb/in³ | ISO 1183 |
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4439 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), and cold rolled strip/sheet forms. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel Characteristics:excellent resistance to general corrosion, excellent resistance to pitting/crevice corrosion, resistant to sensitization, better creep stress-rupture and tensile strength at elevated.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703) Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless s.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® C-300 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Missile components, jet engine shafts. Spring wire for valve springs in high-performance internal combustion engines. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
ATI Allvac® VascoMax® T-200 Specialty Steel Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts.Property values are for samples in the metallurgical condition: 1500°F age.Informat.. |
|||
Density | 8.00 g/cc | 0.289 lb/in³ | |
Crucible Steel REX® M42 High Speed Steel, AISI M42 REX M42 is a super cobalt high speed steel which may be heat treated to HRC 68. This makes REX M42 outstanding for special purpose cutting tools, with requirements beyond the capability of general p.. |