Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.99 g/cc | 0.289 lb/in³ | |
Indium Corp. Indalloy® 162 In-Bi Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.99 g/cc | 0.289 lb/in³ | |
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Density | 7.99 g/cc | 0.289 lb/in³ | |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Density | 7.99 g/cc | 0.289 lb/in³ | |
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Density | 7.99 g/cc | 0.289 lb/in³ | |
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |