Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.88 g/cc | 0.285 lb/in³ | |
Indium Corp. Indalloy® 19 In-Bi-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed Annealed applies to tensile, impact, and hardness values and are for 3/4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of co.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 2 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 3 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 2.4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion res.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Sheet and Strip < 0.1875", UNS S31803 Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded c.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 1 Cold Worked Cold Worked applies to tensile values and are for 0.25" to 4" diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resistanc.. |
|||
Density | 7.88 g/cc | 0.285 lb/in³ | |
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |