Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.87 g/cc | 0.284 lb/in³ | |
Misumi DC53 JIS Tool Steel General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Aluzink 420A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 4D Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® 600DL High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® DC02 (Fe P03) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® DC04 (Fe P04) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Docol® DC06 (Fe P06) Deep-drawing Steel Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Dogal 420YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 024 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 350XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 350YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 490XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | Estimated by MatWeb |
SSAB Tunnplat Domex® 500MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 570, Grade 36 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ASTM A 607 Class 2 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel Hot Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® 255, Grade 37 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® 275, Grade 40 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
ATI Allegheny Ludlum AL 418™ Special (Greek Ascoloy) Martensitic Stainless Steel Uses include engine braces, turbine exhaust components, exhaust struts, stiffeners, and ducts.Information provided by Allegheny Ludlum |
|||
Density | 7.87 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Density | 7.87 g/cc @Temperature 20.0 °C |
0.284 lb/in³ @Temperature 68.0 °F |
|
AK Steel ASTM A 1011, Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F) Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Bake Hardenable (BH 210) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Density | 7.87 g/cc | 0.284 lb/in³ | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Dent Resistant (DR 210) Information provided by AK Steel |