Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.82 g/cc | 0.283 lb/in³ | |
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150 AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.82 g/cc | 0.283 lb/in³ | |
CeramTec Sonox® P51 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |