Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide s.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Latrobe Viscount 44® Prehardened Tool Steel (ASTM H13S) Viscount 44 is a free-machining, prehardened, H13-type hot work tool steel. It is produced using special melting, forging, and heat treating processes which provide the optimum in control
and reprod.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | A |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel CPM® Nu-Die® EZ Tool Steel CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
Density | 7.75 g/cc @Temperature 200 °C |
0.280 lb/in³ @Temperature 392 °F |
hardened to 58 HRC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
Density | 7.75 g/cc @Temperature 199 °C |
0.280 lb/in³ @Temperature 390 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | Semi-Processed and Fully Processed |
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allegheny Ludlum AL 444™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:practically immune to chloride stress corrosion cracking, enhanced resistance to pitting and crevicing, good general corrosi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal Data provided by Allvac.Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Vasco® 440 C UNS S44004 Specialty Steel Uses: Bearing applications including ball bearing assemblies, valve seats and stems, check valve components, bushings.Property values are for samples in the metallurgical condition: 1525FC Quench + .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal Data provided by Allvac.Applications: Rings and structural components for land-based turbines. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® Vasco® X-2M Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization Data provided by Allvac.Applications: High performance helicopter transmission gears, components. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
ATI Allvac® VascoJet® 1000 Specialty Steel, Heat Treatment: 1010°C (1850°F) Q+T Data provided by Allvac.Applications: Landing gear components, springs, fasteners. Gears and shafts for helicopter applications. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Density | 7.75 g/cc @Temperature 400 °C |
0.280 lb/in³ @Temperature 752 °F |
200 HB |
Assab Steels 760 Machinery Steel ASSAB 760 is an easily machinable carbon steel characterized by: Good machinabilityGood mechanical strengthASSAB 760 is primarily intended to be used in the as-delivered condition. It is only to be .. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi.. |
|||
Density | 7.75 g/cc | 0.280 lb/in³ | |
Schmolz + Bickenbach Formadur® 2085 Plastic Mold Steel Description: FORMADUR 2085 is a free-machining corrosion-resistant mold frame steelCharacteristics: Lower mold production costs due to improved machinability; Improved corrosion resistance compared .. |
|||
Density | 7.75 g/cc @Temperature 191 °C |
0.280 lb/in³ @Temperature 375 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |