Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.62 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 12 Chrome Stainless Steel for soft magnetic applications. Information provided by Kinetics, Inc. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
Indium Corp. Indalloy 253 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
Indium Corp. Indalloy 211 Ag-Cu Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
Carlson Nitronic® 60® Austenitic Stainless Steel General DescriptionNitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cob.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 2 Cold Worked Level 2 Cold Worked applies to tensile and hardness properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic all.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |