Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.57 g/cc | 0.273 lb/in³ | |
MarkeTech NB:WO (Sodium Bismuth Tungstate, NaBi(WO4)2) Scintillator Crystal Double tungstate of sodium and bismuth NaBi(WO4)2 (NBWO) is also a new "heavy", "fast" and optically dense oxide single crystal. Is used as a Cherenkov radiator.Data provided by the supplier, MarkeT.. |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
MarkeTech Neodymium Gallium Oxide (NdGaO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 1.2%. |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
Ferro EG 2791 Thick Film Glass Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co.. |
|||
Density | 7.57 g/cc | 0.273 lb/in³ | |
Mateck Neodymium Gallate Substrate, NdGaO3 Substrate single crystals for superconductivity |