Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 88 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 90 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 91 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 92 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 243 Tin Solder Alloy Lead-free alloy, no PatentInformation Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Williams Advanced Alloys WS157 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
American Elements Tin Nanoparticles General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi.. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
AIM 100In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 225 Indium Solder Alloy Information Provided by Indium Corporation |