Density 7.20 - 7.60 g/cc
0.260 - 0.275 lb/in³
Pacific Sintered Materials F-241-T Iron Powdered Metal
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-20All information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials F-241-T Iron Soft Magnetic Powdered Metal
Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE V, CLASS AAll information provided by Pac..
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals.
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals.
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0408-155HTAll information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal
Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials FX-232-T Infiltrated High Carbon Steel Powdered Metal
Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-50All information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal
Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials FX-233-T Infiltrated Alloy Steel
Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals.
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Pacific Sintered Materials FX-233-T(HT) Infiltrated Alloy Steel
Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals.
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal
High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM ..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T Powdered Metal
Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division ..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T(HT) Powdered Metal
Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division ..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T Powdered Metal
Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-50Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated High Carbon Steel FX-232-T(HT) Powdered Metal
Good strength, shock resistance and hardenability, Moderate tolerance control Equivalent MPIF Specification: FX-1008-110HTInformation Provided by Pacific Sintered Metals, a division of PSM Industri..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal
Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Ind..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal
Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind..
Density 7.20 - 7.60 g/cc
0.260 - 0.275 lb/in³
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal
Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 7.20 g/cc
0.260 lb/in³
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy
Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S..
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division..
Density 7.20 g/cc
0.260 lb/in³
Chicago Extruded Metals BioBrass® UNS C62500 Aluminum Bronze
Finished product available in rods.Chicago Extruded Metal temper code: M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Density 7.20 g/cc
0.260 lb/in³
China Tungsten NT6 Titanium Carbide and Nitride Based Carbides
Semi-finishing of low carbon steel, low alloy steel, gray cast iron, Si-AL alloy and finishing of stainless steel.Information provided by China Tungsten
Density 7.20 g/cc
0.260 lb/in³
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze
ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th..
Density 7.20 g/cc
0.260 lb/in³
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G1 contains flake graphite in a matrix that is pearlitic with small amounts of ferrite. This is the softest grade of the Dura-Bar gray irons and is normally selected when excellent machinab..
Density 7.20 - 7.80 g/cc
0.260 - 0.282 lb/in³
China Tungsten ST2175 PM Antifriction Parts
Information provided by China Tungsten
Density 7.20 g/cc
0.260 lb/in³
Anderman Ceramics EREC99 Cerium Oxide
Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met..
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal
DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type V, Class AInformation Provided by Pacific Sintered Metals, a di..