Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.71 g/cc | 0.242 lb/in³ | |
MarkeTech Gadolinium silicate:Cerium (GSO:Ce; Gd2SiO5) Scintillator Crystal Gadolinium silicate doped with cerium is a "fast" crystal and can be used as a protection scintillator. Its possible applications include computer tomography, spatial resolution of less than 1 mm. I.. |