Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
Pacific Sintered Materials BT-121-R Bronze Powdered Metal Applications: Structural and bearing bronze.Equivalent MPIF Specification: CT-1000-K23All information provided by Pacific Sintered Metals. |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
Pacific Sintered Materials SS-316-RD 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Equivalent MPIF Specification: SS-316-40All information provided by Pacific Sin.. |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
Pacific Sintered Materials SS-316-RH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
Pacific Sintered Materials SS-410-R 410 Stainless Steel Powdered Metal Magnetic stainless steel with high strength and good wearing properties.Equivalent MPIF Specification: SS-410-95All information provided by Pacific Sintered Metals. |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RD Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance. Equivalent MPIF Specification: SS-316-40Information Provided by Pacific Sinte.. |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
PSM Industries Pacific Sintered Metals 410 Stainless Steel SS-410-R Powdered Metal Magnetic stainless steel with high strength and good wearing properties Equivalent MPIF Specification: SS-410-95Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.40 - 6.80 g/cc | 0.231 - 0.246 lb/in³ | |
PSM Industries Pacific Sintered Metals Bronze BT-121-R Powdered Metal Structural and bearing bronze Equivalent MPIF Specification: CT-1000-K23Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.40 g/cc | 0.231 lb/in³ | |
China Tungsten NT3 Titanium Carbonitride Alloy Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high corrosion resistance to acids and alkalis and hi-tempe.. |