Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.52 g/cc | 0.163 lb/in³ | Typical |
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Titanium Alloy Medium-Strength Surgical Implant AlloyFeatures: TIMETAL 367 is a dedicated, medium strength, titanium alloy for surgical implants. The alloy was developed specifically for the manufacture of femora.. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 11 Titanium (UNS R52250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550) Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 4 Titanium (UNS R50700) Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402) Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400) Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400) Uses: heat exchangers, industrial components, tubing, CPI equipment.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 7 Titanium (UNS R52400) Uses: CPI equipment, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |