Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.92 g/cc | 0.142 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 625-31 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.92 g/cc | 0.142 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.92 g/cc | 0.142 lb/in³ | |
ICE Al2O3 99.8 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Density | 3.92 g/cc | 0.142 lb/in³ | ASTM C20 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.92 g/cc | 0.142 lb/in³ | |
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |