Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.33 g/cc | 0.120 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 601 Mullite Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e.. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton EXP 338 Alumina 99.6% EXP 338 features high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cyc.. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | |
ICE Hot Pressed SiC Data provided by the manufacturer, International Ceramic Engineering. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | |
Schott N-BAF51 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | ASTM-C20 |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | |
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |
|||
Density | 3.33 g/cc | 0.120 lb/in³ | ASTM-C20 |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |