Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.15 g/cc | 0.114 lb/in³ | |
Poco Graphite SUPERSiC® 3C Silicon Carbide SUPERSiC that has been coated with a 75 µm CVD SiC coating, which seals the surface.Uses: Ideal for high-temperature deposition and CVD applications.Information provided by PocoGraphite |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
Poco Graphite SUPERSiC® 3CX Silicon Carbide SUPERSiC that has been coated twice with a 75 µm CVD SiC coating, which seals the surface. Uses: Ideal for high-temperature anneal processesInformation provided by PocoGraphite |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | Apparent |
Gouda Vuurvast AK 94 M Dense Refractory Brick Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â.. |
|||
Density | 3.15 - 3.25 g/cc | 0.114 - 0.117 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
Schott N-BASF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
TriStar TriSteel PR Metal Backed PTFE Bearing System Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque.. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
TriStar TriSteel PT Metal Backed PTFE Bearing System Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li.. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | ASTM C20 |
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | |
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |
|||
Density | 3.15 g/cc | 0.114 lb/in³ | Apparent |
Gouda Vuurvast LP 85 KP Dense Refractory Brick Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl.. |