Polymer Property : Density = 3.142 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.142 g/cc
0.1135 lb/in³
Advanced Ceramics MEXIM C ACL 2091
Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing applicat..