Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.99 g/cc | 0.108 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0301 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 2.99 g/cc | 0.108 lb/in³ | ISO 1183 |
Eurostar Staramide 6 80E7 PA6, Injection Molded Staramide 6 80E7 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E7)Information provided by Eurostar. |
|||
Density | 2.99 g/cc | 0.108 lb/in³ | |
Ceradyne Ceralloy® 137 CA AlN Composite Applications: cryogenic environment applicationsterminationssever wedgesload pelletsabsorbersFeatures: dielectric loss independent from temperature.Information provided by Ceradyne Company |
|||
Density | 2.99 g/cc | 0.108 lb/in³ | |
Ceradyne Ceralloy® 137 CB AlN Composite Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersFeatures: higher thermal conductivity then Ceraloy® BeO-SiC at temperatures greater then 150°C, cl.. |
|||
Density | 2.99 g/cc | 0.108 lb/in³ | |
Ceramic Process Systems AlSiC-8, 70 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |