Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott N-BAK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott N-SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Alcoa 7055-T7751 Aluminum Plate Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Alcoa 7055-T77511 Aluminum Extrusions Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |
|||
Density | 2.86 g/cc | 0.103 lb/in³ | |
Schott BG20 Band Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BC36 |