Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.21 g/cc | 0.0798 lb/in³ | ASTM D4894 |
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | ASTM D792 |
Manifattura Cattaneo PTFE Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | ASTM 1457-62 T |
Fluorseals PTFE 15% glass filled Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Density | 2.21 g/cc @Temperature 20.0 °C |
0.0798 lb/in³ @Temperature 68.0 °F |
|
Mateck Fused Silica IR Grade (SiO2) Optical crystals |
|||
Density | 2.21 g/cc @Temperature 20.0 °C |
0.0798 lb/in³ @Temperature 68.0 °F |
|
Mateck Fused Silica UV-VIS Grade (SiO2) Optical crystals |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 .. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Vitreosil® 055 Optical Fused Quartz Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | |
Corning Vycor® 7921 UV-Blocking Neodymium Blue Glass Absorbs yellow and UV wavelengths through a process that introduces neodymium and cerium to the glass. Because the elements that create higher color temperature and UV blocking are a art of the gla.. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-S15 PTFE 15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.21 g/cc | 0.0798 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |