Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | ASTM D792 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4894 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4220 PTFE 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 12086 |
3M Dyneon™ TF 2021 PTFE
(discontinued **) Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4895 |
3M Dyneon™ TF 2025 PTFE
(discontinued **) Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 12086 |
3M Dyneon™ TF 2053 PTFE
(discontinued **) Processed by standard paste extrusion methodRecommended grade for extrusion of tubing and cables requiring only moderately high reduction ratioGood overall balance of mechanical properties and proce.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered Sheets; ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Density | 2.15 - 2.18 g/cc | 0.0777 - 0.0788 lb/in³ | DIN 53479 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Apparent |
Gouda Vuurvast A Vuurvast Dense Refractory Brick Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Apparent |
Gouda Vuurvast B 1 Dense Refractory Brick Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
ScanTube PFA Tubing Information provided by ScanTube, Inc. |
|||
Density | 2.15 - 2.19 g/cc | 0.0777 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Density | 2.15 - 2.19 g/cc | 0.0777 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-2 PTFE Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | DIN EN ISO 12086 |
3M Dyneon™ TF 2021Z PTFE Fine Powder Dyneon TF 2021 Z PTFE is an ideal grade for pipe liner applications because of its outstanding green strength. It is the preferred grade for unsintered thread sealing tapes, expanded join sealings, .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | DIN EN ISO 12086 |
3M Dyneon™ TF 2029Z PTFE Fine Powder Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing .. |
|||
Density | 2.15 - 2.30 g/cc | 0.0777 - 0.0831 lb/in³ | |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Density | 2.15 g/cc | 0.0775 lb/in³ | |
Devcon Wear Guard (High Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® E2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® E2 BP PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled