Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Density | 2.12 g/cc | 0.0766 lb/in³ | |
Ferro EG 2790 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,.. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Density | 2.12 g/cc | 0.0766 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.12 g/cc | 0.0766 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di.. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Zeus PFA Tubing PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar.. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Density | 2.12 - 2.17 g/cc | 0.0766 - 0.0784 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Density | 2.12 g/cc | 0.0766 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 25CAR B PTFE; Carbon Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Electrog. Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, .. |
|||
Density | 2.12 g/cc | 0.0766 lb/in³ | ASTM D792 |
Techmer ES HiFill® HIPS 0212 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |