Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6202 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 30-50/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 60-100/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 10-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Density | 2.10 g/cc | 0.0760 lb/in³ | Yield Density |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Apparent |
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | DIN 53479 |
Polyram Metal Cap PPC372B73 Polypropylene, 73% Mineral Filled 73% mineral filled, heavy density polypropylene for molding metallized parts and galvanized coversInformation provided by Polyram Ram On Ind. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina) SiO2 50/ZrSiO4 40/Al2O3 10This form of ceramic is used in the precision foundry industry. The tubes and rods are incorporated into molds in the lost wax process. Using this technique, very fine tole.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Zircar Refractory Composites RS-99W Refractory Sheet Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.Information provided by ZIRCAR R.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Fibre Density |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Cured |
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D1505 |
Arlon CuClad 6700 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%) Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".Information provided by Anderman Cerami.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Arlon AD410 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
BASF Heligoen® Green K 9360 Color Additive Chemical Structure: Cu-phthalocyanine halogenisedApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PETP, CA/CAB, and UPRecommendations for food application.. |
|||
Density | 2.10 - 2.30 g/cc | 0.0759 - 0.0831 lb/in³ | |
Beijing Evergrow Resources PTFE Skived Sheet Tape PTFE resin is first molded into work-blank and then skived. The PTFE resin skived sheet & tape are highly dielectric. Chemical resistant and not aging. They have a wide range of operation temperatur.. |