Polymer Property : Density = 2.0693 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.0693 g/cc
0.074751 lb/in³
Saint-Gobain Chemfab® 10 Anti-Static PTFE-Coated Glass
Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri..
Density 2.0693 g/cc
0.074751 lb/in³
Saint-Gobain Chemfab® 10 Premium PTFE-Coated Glass
Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot..