Physical Properties Metric English Comments
Density 16.2 - 16.6 g/cc
0.585 - 0.600 lb/in³
MarkeTech W85Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
Density 16.2 g/cc
0.585 lb/in³
Wieland 1915 Wilaform Gold
Yield palladium white gold alloy with beautiful grey color. Well suitable for seizing stones.Applications: chains, coin/shape, laminar decoration, tubingDental
Density 16.2 g/cc
0.585 lb/in³
California Fine Wire Alloy 443 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.