Density 16.0 g/cc
0.578 lb/in³
Wieland Porta Maximum PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Density 16.0 g/cc
0.578 lb/in³
Wieland Porta Optimum PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Density 16.0 g/cc
0.578 lb/in³
Williams Advanced Alloys C102 Solder
Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i..
Density 16.0 g/cc
0.578 lb/in³
Goodfellow Gold 75/ Palladium 25 Alloy
Information provided by Goodfellow.
Density 16.0 g/cc
0.578 lb/in³
CMW® ELKONIUM 72 gold based alloy
Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to ..