Density 14.2 g/cc
0.513 lb/in³
Wieland Porta Aurium 2 PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Density 14.2 g/cc
0.513 lb/in³
China Tungsten YG13C Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.2 g/cc
0.513 lb/in³
China Tungsten YG13X Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.2 g/cc
0.513 lb/in³
China Tungsten YT726 Tungsten Carbide
High red hardness and wear resistance. Turning and Milling of chilled cast irons, cast alloy irons and quenched steelInformation provided by China Tungsten