Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.18 g/cc | 0.5123 lb/in³ | |
CMW® ELKONITE® 5W3 Tungsten Copper material ASTM B702, Class C, infiltrated For arcing and current carrying electrical contacts; power transformer contacts.Information provided by CMW Inc. |
|||
Density | 14.18 g/cc | 0.5123 lb/in³ | |
Cadi 5WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |