Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 13.8 g/cc | >= 0.499 lb/in³ | |
Hogen Durakut H15W 68 Tungsten/32 Copper PM Metal Composite RWMA Class ECM-EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che.. |
|||
Density | >= 13.8 g/cc | >= 0.499 lb/in³ | |
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Density | 13.8 - 14.4 g/cc | 0.499 - 0.520 lb/in³ | |
MarkeTech WCu30 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Density | >= 13.8 g/cc | >= 0.499 lb/in³ | |
Mi-Tech Metals CW68 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is recomme.. |
|||
Density | >= 13.8 g/cc | >= 0.499 lb/in³ | |
Mi-Tech Metals CW70E 68 Tungsten/32 Copper PM Metal Composite RWMA Class ECM-EDMMi-Tech Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che.. |
|||
Density | 13.8 g/cc | 0.499 lb/in³ | |
Wieland 1408 Wilaform Gold Hard yellow gold alloy. Easily splintered and polished.Applications: casting, laminar decoration, tubingDental |
|||
Density | 13.8 g/cc | 0.499 lb/in³ | |
Wieland Auropal 2 Casting Alloy Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |
|||
Density | 13.8 g/cc | 0.499 lb/in³ | |
Wieland Portalloy 54 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental |
|||
Density | 13.8 - 14.1 g/cc | 0.499 - 0.509 lb/in³ | |
China Tungsten YG16C Cemented Tungsten Carbide for Mining Purposes For oil cone drill bits for medium soft and medium hard rocks.Information provided by China Tungsten |
|||
Density | 13.8 g/cc | 0.499 lb/in³ | |
China Tungsten ZM15 Tungsten Carbide High in red hardness and strength in use; capable of resistiting high impact load. Semi-finishing or finishing of refractory steel, manganese steel, austenitic stainless steel, machining of cast i.. |
|||
Density | 13.8 - 14.1 g/cc | 0.499 - 0.509 lb/in³ | |
China Tungsten ZY32 Tungsten Carbide for Mining Purposes High toughness and wear resistance, for hi-speed wire mills for intermediate and finish rolling ,able to use for hard wires.Information provided by China Tungsten |
|||
Density | 13.8 - 14.1 g/cc | 0.499 - 0.509 lb/in³ | |
China Tungsten ZY33 Tungsten Carbide for Mining Purposes High toughness and wear resistance, for hi-speed wire mills for intermediate and finish rolling ,able to use for hard wires.Information provided by China Tungsten |