Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.3 - 13.7 g/cc | 0.480 - 0.495 lb/in³ | |
China Tungsten ZC2 Tungsten Carbide Coated substrate with higher toughness and slightly less wear resistance than ZC1, for semi-finishing and roughing after coating.Information provided by China Tungsten |