Polymer Property : Density = 13.2 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density >= 13.2 g/cc
>= 0.477 lb/in³
Hogen H50S, 50 Silver/50 Tungsten PM Metal Composite
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Silver-Tungsten is used when high oxidation-resistant materials are necessar..
Density >= 13.2 g/cc
>= 0.477 lb/in³
Mi-Tech Metals SW50 50 Silver/50 Tungsten PM Metal Composite
Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Silver-Tungsten is used when high oxidation-resistant materials are necessary and s..
Density 13.2 g/cc
0.477 lb/in³
China Tungsten YG640 Tungsten Carbide
Good thermal strength, high resistance to wear, impact and oxidation. Continuous or intermittent cutting of heavy work pieces of cast irons, milling and planning of refractory steel with high streng..
Density 13.2 g/cc
0.477 lb/in³
China Tungsten YT758 Tungsten Carbide
High hardness under high temperature and high wear resistance Continuous or intermittent cutting of steel with super strengthInformation provided by China Tungsten
Density 13.2 g/cc
0.477 lb/in³
CMW® ELKONITE® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress
For electrical ContactsInformation provided by CMW Inc.
Density 13.2 g/cc
0.477 lb/in³
China Tungsten ZM10-1 Tungsten Carbide
High in red hardness and crater resistance .Capable of bearing impact load. finishing of cast iron alloy. mild steel, forgeable nodular cast iron and difficult-to-machine materials such as refractor..