Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183A |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
IDI Composites 44-1 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent moldability and low cost.Data provided by the manufacturer. |
|||
Density | 1.95 - 2.22 g/cc | 0.0704 - 0.0802 lb/in³ | Apparent Density |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | typical |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D572 |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | DIN 53479 |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Applied Composites 8052 Polyester SMC Industry Application: RecreationProduct Application: Marine ProductsDistinct Features: High Strength, ResilientInformation provided by Applied Composites Corporation. |
|||
Density | 1.95 - 2.15 g/cc | 0.0704 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Zircar Ceramics AL-CEM Alumina Cement Type AL-CEM Alumina Cement is a high purity alumina bonding agent used for bonding ZIRCAR® fibrous ceramic products to themselves, and as a coating cement to improve the hardness and oxidation resi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183A |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8805 is a vinyl ester-based sheet molding compound (SMC) reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness, and fatigue resistance in the fiber .. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |