Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
IDI Composites E-203 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
SGL Carbon Group EK 2200 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
SGL Carbon Group EK 2201 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C30 S003 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Fiber Density |
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® Z03 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Plenco 5118 Phenolic, Granular, Injection Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ASTM D792 |
Plenco 7556 Phenolic, Briquette, Injection Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Relative Density; ISO 1183 |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | ISO 1183 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | |
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.82 g/cc | 0.0658 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |