Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792A |
Resinoid 1363 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional .. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF) Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically .. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | Stand relative density |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Plenco 6401 Phenolic, Granular, Compression Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Toho Tenax Besfight® STS 24K HTA-7C F301 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Zoltek Panex 35® Milled Carbon Fibers Milled Carbon FibersApplications include: Buoyancy, RFI/EMI Shielding, Static Dissipation, Surface Reinforcement, Low Cost Polyurethane Friction Compounds |
|||
Density | 1.75 g/cc @Thickness >=0.000 mm |
0.0632 lb/in³ @Thickness >=0.000 in |
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3 |
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NT40 GR60 NL HS PPA, 60% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
DSM Arnite® AV2 365 SN PET-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Brandenburger BL 20/1 GG EP Rotor Blade Material BL 20/1 GG EP is a composite bearing material that combines the crucial parameters for rotary blades. These include compressive stability at high temperatures, impact strength, low swelling and low.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Density | 1.75 - 1.95 g/cc | 0.0632 - 0.0704 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Toho Tenax Besfight® G30-500 12K HTA-7S F202 Continuous Filament Carbon Fiber Standard Modulus; Soft Wide Band; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |